LOCTITE EDAG 33RO65A

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE EDAG 33RO65A

Main features

  • High-Speed Conductive Printing
  • Graphite-Polyimide Temperature Stability
  • Low-Resistance Printed Conductivity

Product Description

LOCTITE EDAG 33RO65A is a black, graphite-filled polyimide conductive coating for high-speed printing. The heat-cured paste is formulated for adhesion to multiple substrates and produces a conductive printed layer with sheet resistance below 20 ohms/sq/mil under the stated cure. A staged schedule of 20 minutes at 107 deg C followed by 60 minutes at 177 to 204 deg C develops the polyimide coating for elevated-temperature stability. Applications include conductive printed coatings and ink features where this graphite/polyimide system is specified.

Key features

  • Graphite-polyimide construction: The conductive coating combines graphite filler with a polyimide binder.
  • High-speed printability: The paste is formulated for high-speed printing equipment.
  • Staged heat cure: The documented two-stage cure develops a low-resistance conductive layer.

Applications

Applications include high-speed printed conductive coatings and ink features where EDAG 33RO65A is specified.

Product Family

LOCTITE EDAG 33RO65A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Black paste
Chemistry Type Chemistry Type
Polyimide
Density (g) Density (g)
1.12 g/cm3
Solids Solids
22 %
Physical Properties
VOC VOC
876 g/l
Thermal Properties
Flash Point Flash Point
>60 to 77 °C

Additional Information

Technical properties

As-supplied properties

Typical uncured and processing values.

Property Value Unit Method / condition
AppearanceBlack pasteAs supplied
TechnologyPolyimideBinder system
Filler typeGraphiteConductive filler
Solids content22%By weight
Density1.12kg/lUncured material
Theoretical coverage265sq ft/gal/milUncured coating
Shelf life365daysAt 2 to 8 deg C in original seal
Cure schedule20 minutes at 107 deg C plus 60 minutes at 177 to 204 deg CGuideline heat cure