DCT-PVC95 | Polymerized Vinyl Chloride Dicing Tape

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

DCT-PVC95 | Polymerized Vinyl Chloride Dicing Tape

Main features

  • 95 µm film thickness
  • UV removable acrylic adhesive
  • Strong adhesion for silicon wafer applications

Product Description

LINQTAPE™ DCT-PVC95 is a polymerized vinyl chloride tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Its strong adhesion ensures the wafer remains secure during different manufacturing processes like die-cutting.  The security the tape provides prevents wafer damage, whiskers, soaking and allows for cleaner cuts. 

LINQTAPE™ DCT-PVC95 can be peeled by using UV. To ensure a clean substrate after removing the tape, DCT-PVC95 utilizes a technology through which after applying UV light, the adhesive (3,200 N/25mm) becomes less tacky (140 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass, sensitive substrates, and applications for which the final product must be clean of any residue. DCT-PVC95 is a translucent 80µm film, with a one-sided 15µm acrylic adhesive layer, and backed with a PET liner. It is ideal for small chips. 

Key Features

  • Strong adhesion to prevent wafer damage
  • UV removable adhesive
  • No residue
  • Can be used with uneven surfaces
  • Antistatic
  • High Transparency
  • High and evenly distributed elasticity 
  • High heat tolerance (60 °C for a few minutes)

Application Ideas

  • Die -cutting
  • Glass and sensitive applications 
Product Family

LINQ DCT-PVC95

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Acrylic
Adhesive Thickness Adhesive Thickness
15 µm
Appearance Appearance
Translucent
Film Thickness Film Thickness
80 µm
Release Liner Release Liner
PET
Total Thickness Total Thickness
95 μm
Mechanical Properties
Adhesion Strength Adhesion Strength
10790 Oz/in
Elongation Elongation
320 lengthwise, 340 crosswise %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
31 lengthwise, 25 crosswise N/cm