DCT-PO200 | Polyolefin Dicing Tape

Harmonization Code : 3920.10.89.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials; Of polymers of ethylene; Of a thickness exceeding 0,125 mm; Other; Other; Other

DCT-PO200 | Polyolefine Die Cutting Tape

Main features

  • 200 µm film thickness
  • UV removable acrylic adhesive
  • Gentle adhesion for packaging substrates and glass

Product Description

LINQTAPE™ DCT-PO200 is a frosted polyolefin (PO) tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Compared to a PET dicing tape, PO dicing tapes have the same strong adhesion but are more easily removed from the substrate. This makes it ideal for applications such as packaging substrates, or delicate substrates where gentler adhesion is required for easier removal. DCT-PO200 is a higher viscosity formulation compared to DCT-165, providing the tape with higher moisture, heat, and environmental resistance. Higher viscosity also increases the adhesion strength of the tape. 

LINQTAPE™ DCT-PO200 can be peeled by using UV. To ensure a clean substrate after removing the tape, DCT-PO200 utilizes a technology through which after applying UV light, the adhesive (23,000 N/25mm) becomes less tacky (200 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass, sensitive substrates, and applications for which the final product must be clean of any residue. DCT-PO200 is a 150µm PO film, with a one-sided 50µm acrylic adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

LINQ DCT-PO200

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Acrylic
Adhesive Thickness Adhesive Thickness
50 µm
Appearance Appearance
Frosted
Film Thickness Film Thickness
150 µm
Release Liner Release Liner
PET
Total Thickness Total Thickness
200 μm
Mechanical Properties
Adhesion Strength Adhesion Strength
82735 Oz/in
Elongation Elongation
903 lengthwise, 867 crosswise %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
34 lengthwise, 31 crosswise N/cm

Leading Brands Trust in Our Products and Services