HUMISEAL 1B31/521 Acrylic Conformal Coating

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

HUMISEAL 1B31/521

Main features

  • 65 +/- 5 cP Preblend
  • Fast-Drying Moisture Protection
  • Strong Cured Electrical Properties

Product Description

HumiSeal®1B31/PB25 Acrylic Conformal Coating is a fast-drying, single-component acrylic conformal coating pre-blended to a viscosity suitable for immediate use. Designed for printed circuit assemblies, it provides moisture and environmental protection while maintaining excellent flexibility. The coating fluoresces under ultraviolet light for inspection, is easily repairable, and develops cured properties comparable to standard HumiSeal® 1B31.

Key features

  • Ready-to-use viscosity: Supplied pre-blended for immediate application without the need for additional dilution.
  • Moisture and environmental protection: Protects printed circuit assemblies from moisture and environmental exposure.
  • Flexible and repairable: Produces a flexible coating that can be readily repaired when required.
  • UV inspection: Fluoresces under ultraviolet light to assist coating coverage inspection.

Applications / Suitable for

  • Conformal coating of printed circuit assemblies
  • Applications requiring moisture and environmental protection
  • Dip, spray, or brush coating processes using a compatible pre-blend viscosity
Product Family

HUMISEAL 1B31/521

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Thickness range Thickness range
0.025-0.075 mm
Thermal Properties
UL 94 Rating UL 94 Rating
V-0
Electrical Properties
Breakdown Voltage Breakdown Voltage
7,500 V

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-coating and processing properties for HumiSeal® 1B31/521. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product form Single-component acrylic conformal coating pre-blend — As supplied; specifically diluted for immediate use
Viscosity 65 ± 5 cPs As supplied
Solids content 24 ± 1 % As supplied
Density 0.90 ± 0.02 g/cm³ As supplied
VOC 685.8 g/L As supplied
Drying time to handle 10 minutes Fed-Std-141, Method 4061
Recommended curing conditions 24 hours or 30 minutes — 24 hours at room temperature or 30 minutes at 76°C
Time to optimum properties 7 days After application
Shelf life 24 months From date of manufacture; store tightly closed at 0 to 35°C
Technical properties

After-processing / final-state properties

Typical cured properties shared by HumiSeal® 1B31 and its pre-blends. Values are not intended for use as specifications.

Property Value Unit Method / condition
Recommended coating thickness 25–75 microns Cured coating
Thermal shock 50 cycles — MIL-I-46058C; −65°C to 125°C
Coefficient of thermal expansion, below Tg 170 ppm/°C TMA
Coefficient of thermal expansion, above Tg 340 ppm/°C TMA
Glass transition temperature 14 °C DSC
Modulus at −40°C 2000 MPa DMA
Modulus at 20°C 1050 MPa DMA
Modulus at 60°C 8.5 MPa DMA
Flammability Self-extinguishing — MIL-I-46058C
Dielectric withstand voltage >1500 volts MIL-I-46058C
Dielectric breakdown voltage 7500 volts ASTM D149
Dielectric constant 2.5 — ASTM D150-98; 1 MHz and 25°C
Dissipation factor 0.01 — ASTM D150-98; 1 MHz and 25°C
Insulation resistance 8.0 × 1014 (800 TΩ) ohms MIL-I-46058C
Moisture insulation resistance 6.0 × 1010 (60 GΩ) ohms MIL-I-46058C
Fungus resistance Passes — ASTM G21