DOWSIL 738 ELECTRICAL SEALANT

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

DOWSIL 738 ELECTRICAL SEALANT

Main features

  • One-Part Moisture-Cure Sealing
  • Non-Sag Placement Control
  • 500% Cured Elongation

Product Description

DOWSIL™ 738 Electrical Sealant is a one-part, white, non-flowing moisture-cure silicone adhesive and sealant for bonding and sealing electrical assemblies. It cures at room temperature without component mixing or oven curing and can be heat-accelerated when faster in-line processing is required. The cured elastomer combines 500% typical elongation with Shore A 35 hardness, providing flexibility and stress relief in electrical components, circuit boards, assemblies and housings.

Key features

  • One-part moisture cure: Requires no component mixing and cures at room temperature without an oven.
  • Non-flowing consistency: Supports controlled application and placement during bonding and sealing operations.
  • Flexible cured elastomer: Provides 500% typical elongation for stress relief in electrical assemblies.

Applications / Suitable for

  • Bonding and sealing electrical assemblies
  • Circuit boards and assembled electronic systems
  • Electrical components and housings
  • Battery-pack assembly applications
Product Family

DOWSIL 738

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity Specific Gravity
1.04
Physical Properties
Viscosity Viscosity
Non-flowing mPa.s
Mechanical Properties
Elongation Elongation
500 %
Physical Properties
Tack-Free Time Tack-Free Time
89 minutes
Electrical Properties
Dielectric Strength Dielectric Strength
19 kV/mm
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.2 W/m.K
Mechanical Properties
Peel Strength Peel Strength
16.5 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical characteristics of the sealant before cure. Typical values are not intended for use as specifications.

Property Value Unit Method / condition
Color White — As supplied; typical
Flow characteristic Non-flowing — As supplied
Specific gravity 1.04 — At 25°C; typical
Tack-free time 89 minutes At 50% relative humidity; typical
Cure system Moisture cure — One-part, room-temperature cure; optional heat acceleration
Technical properties

After-processing / final-state properties

Typical properties of the cured silicone elastomer. Typical values are not intended for use as specifications.

Property Value Unit Method / condition
Durometer hardness 35 Shore A Cured material; typical
Elongation 500 % Cured material; typical
Tensile strength 360 psi Cured material; typical