Chemlinq MRE-C909 Mold Release is a carnauba wax based, sprayable aerosol mold release agent. It contains no silicones or oils and is therefore not only compatible but complementary to epoxy molding compound and other thermoset plastic molding.

Alternative to MJGordon Permasil #909C

Chemlinq MRE-C909 is a fully REACH and RoHS compliant carnauba wax mold release aerosol spray and does not contain trichloroethane (CAS: 71-55-6) or dichloromethane (CAS: 75-09-02). It is designed for mold release of epoxy molding compounds and was specifically formulated as an alternative to MJ Gordon Permasil #909C after MJ Gordon discontinued the production of this product. MRE-C909 is literally the 9th iteration, and serves as a reminder of the 8 previous unsuccessful formulation attempts before finally formulating MRE-C909.

In order to have the best results during the production process, a thin, uniform thickness of MRE-C909 should be sprayed on the mold. The release agent has no build-up on the mold and should show a shiny surface when properly applied.

Instructions for use:

  1. Frequently shake the container to agitate the wax which has the tendency to fall to the bottom of the can. (Note: Carnauba wax has a greater density than the solvents and propellant in the formulation)

  2. Hold the container upright with the actuator (spray nozzle)  pointing toward a red mark on the mounting cup of the valve.

  3. Press the actuator to discharge the wax, from a distance of at least 30 cm from the mold surface, moving the container side to side.(Note: If you spray at the same spot for more than 2 sec, then you might overspray the mold surface with uneven wax)

General Notes:

  1. If the spray actuator is too close to the surface, water condensation will happen on the mold surface and will cause contamination on the molded product.
    Spray distance of 30 cm will allow the evaporation of the solvent and propellant and will eliminate the condensed water vapor in the air.
  2. To ensure consistent formulation during use, MRE-C909 is only available in aerosol cans.

 

Product Family

CHEMLINQ MRE-C909

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Milky Wax Solution
Auto ignition temperature Auto ignition temperature
237 °C
Chemistry Type Chemistry Type
Carnauba Wax
Evaporation Rate Evaporation Rate
1.5
Specific Gravity 250°C Specific Gravity 250°C
0.69 g/cc
Vapor Density Vapor Density
2.3
Vapor Pressure Vapor Pressure
3.8 kg/cm2

Additional Information

MRE-C909 Development, Performance and Applications

Carnauba wax itself is nothing new. It is a natural wax derived from the a palm tree native to the northeastern Brazil. It is used in a wide variety of applications including automotive waxes, shoe polishes, dental floss coatings, and paper coatings. More importantly, it is used in the production of epoxy molding compounds themselves as the mold release agent.

Carnauba wax is the same natural mold release wax used in the manufacture of semiconductor epoxy molding compounds.

In mold release applications, carnauba wax is used because of its excellent release properties. It creates a thin and uniform coating on the mold surface, allowing the material to be released cleanly without sticking to the mold.

Teflon, silicone, and oils are all used as mold release agents, but none of them is as well suited to thermoplastic mold release as carnauba wax.

There is no silicone, Teflon or oil in the MRE-C909 formulation. While Teflon and silicone may be well-suited for rubber, they rarely have a place when working with liquid epoxy or epoxy molding compounds (EMC). Most semiconductor manufacturers use chunks of carnauba wax to break in new molds; MRE-C909 provides this same compatibility in a convenient, high-purity spray.

Carnauba Wax is the best mold release for optically clear mold compounds

REACH & RoHS Compliant: Chemlinq MRE-C909 does not contain chlorofluorocarbons, ozone-depleting substances, trichloroethane, or dichloromethane.

Clear epoxy releases cleanly with MRE-C909 Carnauba Wax

Chemlinq MRE-C909 is a non-silicone mold release agent developed specifically for transfer molding and compression molding. It is ideal for applications requiring a thin, uniform layer for best results. Due to its dryness, MRE-C909 provides the perfect balance of release and rustproofing.

Tips & Troubleshooting

  • Shake the aerosol can frequently to avoid clogging.
  • Maintain distance to ensure the required spray pattern.
  • Spray evenly and quickly during production. Do not overspray.
  • Used to rust proof metal molds while they are still hot.

Alternative for MJ Gordon Permasil #909C

Chemlinq MRE-C909 is a proven alternative to MJ Gordon #909C. This carnauba wax-based spray is fully REACH and RoHS compliant. Just like the MJ Gordon version, it is an aerosolized solution of carnauba wax suspended in solvent. However, our compliant solvent and propellant ensure it can be used in European markets where legacy products are restricted.

Evaluation of Mold Release Products

Semiconductor Grade Epoxy Molding Compound was tested with 5 different candidates

Incompatible Candidates

  • Did not dry during the molding cycle
  • Caused increased sticking in the mold
  • Visual defects in molded bars were observed
  • Offensive odor; burning eyes and irritation
Incompatible Candidate

Chemlinq MRE-C909 Results

  • Processed equally well as MJ Gordon #909C
  • No sticking or operator irritation
  • Identical results to legacy benchmarks
  • Very good release properties
Compatible Candidate
Innovation Insight

Design Features & Uniformity

Red Dot

Why is there a red dot?

 

The red dot is a "spray-through" indicator. It aligns the nozzle with the internal valve stem. By pressing down until the dot disappears, you ensure the spray can is being used efficiently with zero wasted product.

Propellant

Why is there no "metal pea"?

 

MRE-C909 uses a modern solvent and propellant mixture that ensures proper homogeneity without an agitator ball. This REACH-compliant formulation stays blended, eliminating the need for a mixing ball.

Product Cross-Reference

Alternatives & Compliance

There is no direct alternative for this product; rather, Chemlinq MRE-C909 is the engineered, REACH-compliant alternative to MJ Gordon Permasil #909C.

 

Package Size Availability

To ensure consistent formulation during use, MRE-C909 is only available in aerosol cans.

Technical Support

Guidelines for Troubleshooting Common Issues

Defect Description Corrective Action
Mold Sticking
  • Increase mold temperature and preheat material to eliminate moisture.
  • Clean the mold and check for dents or undercuts.
  • Ensure cavities have sufficient draft for easy removal.
Porosity / Voids
  • Increase molding pressure and experiment with different plasticity levels.
  • Reduce temperature and adjust closing speed to purge air.
Blistering
  • Increase cure time and vent the mold at dead ends.
  • Close mold slowly on low pressure first to allow gas to escape.
Material Compatibility

Carnauba Wax Compatibility Chart

Measured as % of Material Properties Retained (Tensile Strength & Displacement)

Highly Compatible (A)

90-100+% Property Retention

  • Epoxy
  • Acetal
  • PET
  • PPS
  • ABS

Moderate (B)

80-89% Property Retention

  • Polyethylene
  • PEI
  • PPO

Not Compatible (C)

Less than 80% Retention

  • Acrylic
  • Polycarbonate
  • Polypropylene
  • SBR Rubber

Note: This data is intended as a guide; specific applicability must be ascertained through product testing within particular manufacturing conditions.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers