BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other
Main features
- Ready-to-Use Touch-N-Prep Pen
- No-Rinse Dry-in-Place Processing
- Modifiable Felt-Tip Applicator
Product Description
BONDERITE® M-CR 1132 AERO Touch-N-Prep® Pen is a ready-to-use hexavalent chromium conversion coating applicator for localized touch-up and repair of aluminum and aluminum-alloy surfaces. The dry-in-place treatment is applied directly from the pen without rinsing and may be air-dried or force-dried with warm air. Its controlled felt-tip delivery system supports treatment of edges, holes, rivets, and other small or difficult-to-reach areas while reducing chemical use, worker contact with chromating solutions, and rinse-water waste compared with conventional chromating processes.
Key Features
- Ready-to-use conversion coating: Delivers a dry-in-place hexavalent chromium treatment directly from the applicator pen without mixing or dilution.
- No-rinse application: The applied coating can be air-dried or force-dried with warm air at a maximum recommended temperature of 60°C (140°F).
- Controlled touch-up delivery: The felt-tip applicator supports localized treatment of edges, holes, rivets, and other small or difficult-to-reach aluminum surfaces.
Applications / Suitable for
- Touch-up and repair of conversion coatings on aluminum and aluminum-alloy surfaces
- Localized treatment of bare areas on aircraft and aircraft-part surfaces
- Treatment of edges, rivets, holes, and other small or difficult-to-reach areas
Technical Specifications
General Properties
Additional Information
After-Processing / Final-State Properties
Typical coating-weight and coverage guidance when two coats are applied.
| Property | Value | Unit | Method / Condition |
|---|---|---|---|
| Light Coating Weight | 13 to 18 | mg/ft² | Class 1A and Class 3; two coats; approximately 50 ft² coverage per pen |
| Moderate Coating Weight | 18 to 22 | mg/ft² | Class 1A and Class 3; two coats; approximately 35 ft² coverage per pen |
| Heavy Coating Weight | 22 to 35 | mg/ft² | Class 1A only; two coats; approximately 25 ft² coverage per pen |
| Minimum Double-Coat Weight | At least 10 | mg/ft² | When the applicator pen adequately wets the surface |